冷再生施工和机械租赁业务
筑路架桥,奉献社会;以人为本,不断创新

服务热线

18264104888

新闻中心

首页>>新闻中心冷再生机施工中如何处理接缝问题?

冷再生机施工中如何处理接缝问题?

来源:http://www.tclqgc.com/ 日期:2023-06-12 发布人:
路面的接缝问题就是冷再生机在对道路进行施工中停机所导致的,每次停机,哪怕只是停机几分钟用于更换罐车,也会造成路面再生材料铺设的横缝,缝隙的产生会影响到接下来再次施工时的材料的均匀性。因此在施工的过程中应当尽量避免停机,事不可为的话,应当及时的对缝隙进行处理。下面冷再生机出租厂家就来讲解一下如何处理接缝问题。
The joint problem on the road surface is caused by the shutdown of the road during the construction of the cold reinvigoration process. Even if the shutdown is only for a few minutes to replace the tank truck, it can cause transverse joints in the laying of recycled materials on the road surface. The generation of cracks will affect the uniformity of the materials during the subsequent construction. Therefore, during the construction process, it is necessary to avoid downtime as much as possible. If things cannot be done, the gaps should be dealt with in a timely manner. Below, the rental manufacturer of the cold regeneration machine will explain how to handle the seam problem.
1、在临时停机后重新开始施工时,整个再生机组应倒退1.5~2m的距离到达再生过的材料上,以保证开始施工后所有材料均得到处理。
1. When resuming construction after a temporary shutdown, the entire regeneration unit should be backed up by a distance of 1.5-2m to reach the recycled material, to ensure that all materials are processed after starting construction.
2、上一作业段压实时,要预留4~6m不进行碾压,待下一段碾压时一并压实。
2. During the compaction of the previous operation section, a distance of 4-6 meters should be reserved for no compaction, and the next section should be compacted together.
冷再生机出租
3、由于再生机开始工作时要使转子全部下切到再生层的底部来打碎再生料,前进速度为0,使得翻松的再生料混合不均匀,为此,需人工进行翻拌后将坑槽找平。
3. Due to the fact that when the regeneration machine starts working, it needs to cut all the rotors down to the bottom of the regeneration layer to break the recycled material, with a forward speed of 0, resulting in uneven mixing of the loosened recycled material. Therefore, it is necessary to manually mix and level the pit.
再生机的工作宽度一般要小于再生路面的宽度。因此,全幅路的再生需要多次作业,从而导致数条相邻作业面间的纵向接缝。
The working width of the recycling machine is generally smaller than the width of the recycled road surface. Therefore, the regeneration of the full width road requires multiple operations, resulting in longitudinal joints between several adjacent working surfaces.
一般来讲,相邻作业面间的小重叠量为10cm,以保证纵缝处再生料的连续性,同时避免相邻作业面间存在未再生的夹带。更多相关事项就来我们网站http://www.tclqgc.com咨询!
Generally speaking, the small overlap between adjacent working surfaces is 10cm to ensure the continuity of recycled material at the longitudinal joint, while avoiding the presence of unrecycled entrainment between adjacent working surfaces. For more related matters, come to our website http://www.tclqgc.com consulting service

阅读/ Recommended reading

WR530V路面冷再生机是我公司新推出的路面冷再生机,这款产品不同于450和450机型,是一款完全胜任水稳路基冷再生施工的经济型冷再生机,主要技术参数向600机型看齐,产品综合性...

WR2100L冷再生机转子双转速的应用 2024-04-21
沥青路面养护为什么要使用冷再生机? 2024-04-21
你不知道的压路机选型要点 2024-04-11
旧沥青路面冷再生机械如何进行施工? 2024-04-09

产品/ Recommended products